Cooling Precision Equipment Without Inviting Silicone Contamination

Date:2026-11-04 

In an industrial camera, a precision instrument, or an optical communication module, cooling is never just a temperature story. Yes, the chip needs to stay within its thermal budget. But the optical window also needs to stay clear, the contacts need to stay reliable, and the assembly needs to survive without bending a thin PCB or stressing a delicate package.

 

That is where a thermal pad can quietly solve one problem and introduce another. A datasheet may promise excellent conductivity, while volatiles, surface migration, or compression load create a fresh batch of unknowns elsewhere in the device. Not exactly a fair trade.

Sheen's AF Series takes a different route. AF500, AF800, and AF1000 use a non-silicone base system designed without intentionally added silicone oil or siloxane components, reducing one potential source of silicone contamination. Their nominal thermal conductivities are 3.0, 8.0, and 10 W/(m·K), respectively, and custom die-cutting lets the pad match the actual assembly rather than forcing the assembly to accommodate a rectangle.

 

Die-cut AF Series product examples

Figure 1. Die-cut AF Series product examples. Shapes can be customized to the assembly; the image does not represent one specific grade.

 

Why “Non-Silicone” Matters Near Optics and Contacts

Silicone thermal pads have a long, well-established track record. This is not a story about a material category suddenly becoming the villain. The point is narrower and more practical: near lenses, optical windows, precision contacts, or relays, a non-silicone material gives engineers another way to control a specific contamination pathway.

Omron's relay usage precautions describe the mechanism clearly. Gas emitted by surrounding silicone materials can form silicon oxide on relay contact surfaces and contribute to poor electrical contact. It is less ‘smoke and fireworks,’ more slow-motion contamination — easy to miss during a short bench test, much harder to excuse after field failures appear.

The AF Series combines a non-silicone base formulation with gap filling and die-cut positioning, making it a sensible candidate for comparison in these projects. But the wording matters, so let's put three boundaries on the table:

  • “Non-silicone” describes the base material system. It does not mean the material contains no silicon element at all.
  • “Zero siloxane” is a formulation position. A ‘not detected’ result for specified siloxanes must always travel with the test method and detection limit.
  • Low bleed and low volatility must be verified for the specific grade and agreed test conditions. Neither means absolute zero contamination or zero emission under every possible condition.

 

Meet the AF Series: Three Conductivity Levels, Three Different Jobs

AF500 is the starting point for general gap filling. AF800 steps up when the first option cannot meet the thermal target at the same thickness and assembly conditions. AF1000 pushes nominal conductivity further for designs that need to reduce bulk material resistance within a 0.5–2 mm thickness range.

That sounds simple enough. The trick is to choose with conductivity, thickness, compressed contact, and cleanliness requirements in the same frame — not to crown the biggest number before checking the interface.

 

PropertyAF500AF800AF1000
Thermal conductivity, W/(m·K)3.0 ± 0.38.0 ± 0.810 ± 1
Thickness, mm0.5–50.5–50.5–2
ColorWhite / grayGrayGray
Density, g/cm³2.8 ± 0.23.3 ± 0.23.3 ± 0.3
Hardness, Shore 0055 / 707070 ± 8
Operating temperature, °C−40 to 125−40 to 125−40 to 125
AC breakdown voltage, kV≥8≥8≥4
Volume resistivity, Ω·cm (250 V test)≥10¹²≥10¹¹≥10¹¹
Thermal resistance, °C·in²/W≤0.5 @30 psi≤0.4 @30 psi≤0.13 @50 psi

Table 1. Source: AF500 and AF800 TDS version 20260402V0; AF1000 TDS version 20260327V1.

Where Each Grade Fits

  • AF500 — start here for general gap filling and moderate heat loads on precision control boards. Compare the 55 and 70 Shore 00 options for contact and assembly load before deciding whether 3.0 W/(m·K) meets the temperature target.
  • AF800 — use it as the 8.0 W/(m·K) comparator when AF500 falls short at the established thickness and assembly conditions. The real gain still depends on contact resistance, compression, and the rest of the cooling path.
  • AF1000 — evaluate it for higher-conductivity needs in the 0.5–2 mm range. Compare it with AF800 at the same thickness and assembly conditions to see whether the 10 W/(m·K) grade delivers the temperature improvement the project actually needs.

 

Conductivity Helps — but the Interface Gets the Final Vote

 

Sheen AF series non-Silicone Thermal pad thermal conductivity values and stated tolerances

Figure 2. TDS thermal conductivity values and stated tolerances for the three grades. Test method: ASTM D5470

A Quick R = t/(kA) Reality Check

For one-dimensional steady-state conduction through the pad itself, use R = t/(kA), where t is thickness, k is thermal conductivity, and A is effective heat-transfer area. With thickness and area held constant, a higher k lowers bulk resistance. Simple enough. The real interface, however, also includes contact resistance on both sides and responds to flatness, assembly pressure, and compressed thickness.

Here is a design calculation, not a measured system result. Assume a 1.0 mm actual pad thickness, a 20 × 20 mm effective area, uniform heat flow of 10 W, and only the nominal conductivity of each grade.

 

Calculated ItemAF500AF800AF1000
Theoretical bulk thermal resistance, K/W0.8330.3130.250
Theoretical temperature difference across the pad, °C8.333.132.50

Table 2. Idealized calculation only. It excludes contact resistance, spreading resistance, and heatsink resistance. It is not a measured system result and must not be read as a promised chip-temperature reduction.

Thickness and Contact Can Reshape the Comparison

Consider AF1000 at 2 mm and AF500 at 0.5 mm. You cannot rank their area-normalized bulk resistance by conductivity alone; thickness has changed at the same time. Match the real gap first, then choose the smallest reasonable thickness that still provides reliable contact. That usually does more good than chasing conductivity in isolation.

AF pads offer self-adhesive positioning and custom die-cutting, which helps when installing around chips, housings, or metal spreaders. But hardness is not a compression-force curve. For thin PCBs, optical brackets, and sensitive packages, verify reaction force across the assembly tolerance range. If an additional adhesive layer is added, evaluate its effect on both thermal resistance and emissions as well.

 

Pressure, Gap and Tolerance: The Mechanical Side of Thermal Design

The load your structure can tolerate determines the condition in which the pad is allowed to work. The 30 psi and 50 psi values in the TDS belong to the corresponding thermal-resistance measurements. They are not mandatory assembly pressures, and they are definitely not a compression-reaction curve.

 

Pressure-to-load conversion at the loaded interface

 

Figure 3. Pressure-to-load conversion for a uniformly loaded 20 × 20 mm interface, calculated as F = P × A. These are geometric calculations, not AF material compression measurements.

 

At 30 psi — about 207 kPa — a 20 × 20 mm interface carries roughly 82.7 N. At 50 psi, about 345 kPa, the load rises to roughly 137.9 N. Whether the package, PCB, bracket, fasteners, and load path can tolerate that force is a structural question. If your assembly can only provide lower pressure, compare interface resistance and contact condition at that lower pressure instead of borrowing the high-pressure datasheet result.

Compression Must Cover the Real Assembly Tolerance

Estimate geometric compression as ε = (t₀ − g)/t₀, where t₀ is initial pad thickness and g is the assembled gap. If the gap varies from 0.8 to 1.0 mm, an ideal 1.0 mm pad sees 0–20% geometric compression. At the maximum gap, it may have no preload at all; at the minimum gap, reaction force needs a close look. And this simple example has not even included pad-thickness tolerance yet.

For a real specification, calculate pad-thickness tolerance together with the minimum and maximum structural gaps. Then check reaction force, recovery, and compression set at the relevant temperature and compression. AF500's 55 and 70 Shore 00 options are useful comparison points, but hardness values cannot substitute for those measurements.

An Industrial Camera Example

For a ‘processor — thermal pad — metal housing’ path, record the chip temperature point, housing temperature, and image-focus stability together. Keep power, ambient conditions, housing cooling, and measurement methods consistent across samples, and evaluate the parts in their actual assembled state. This is a validation method example, not a reported AF Series customer installation.

 

Where the AF Series Fits

Optical Modules and Precision Optical Equipment

Optical modules, industrial cameras, and precision imaging devices often pack heat-generating chips and optical components into the same tight space. Heat needs a clean path to the metal housing, while lenses, windows, and coupling areas need protection from condensable contamination. That combination gives non-silicone thermal pads a clear reason to be evaluated.

 

Optical module internal structure

 

Figure 4. Optical module structure showing the transmitter, receiver, IC, and other elements. Source: Sheen application presentation [2]. This illustration does not indicate qualification by any specific customer.

 

AF1000 is a candidate for concentrated heat sources with short chip-to-housing paths. AF800 suits areas that need both gap filling and higher conductivity, while AF500 can serve lower-heat control or auxiliary circuits. Check the available space near optical parts, assembly pressure, and whether the compressed pad could intrude into an optical path or connection area.

Industrial Control and Medical Electronics

In industrial vision controllers, precision instruments, and the control or processing units of medical imaging equipment, AF pads can be evaluated between main processors, FPGAs, memory, power devices, and the enclosure. Reducing silicone contamination sources is especially relevant when relays, precision connectors, or optical sensors share the structure.

General control and acquisition boards can start with AF500; hotter processing or power locations can compare AF800 and AF1000. For medical electronics, this discussion is limited to thermal components inside the equipment. Material selection still belongs within the device's electrical-safety, cleaning, and compatibility validation. Nothing here implies patient contact, implantation, or biocompatibility claims.

Optical cleanliness tests should define temperature, time, and the condensing surface. Vacuum or high-cleanliness projects may also evaluate TML and CVCM where required. ASTM E595, as described by NASA, is a vacuum-outgassing evaluation method — not a certification already obtained by the AF Series.

Laptops and Compact Computing Devices

SSD controllers, memory packages, power components, and auxiliary chips in laptops often conduct heat through pads to shields, thermal modules, or the enclosure. AF500 is a starting candidate for ordinary gaps and heat loads; AF800 and AF1000 can be compared where localized hotspots need a stronger conduction path.

Thin devices add more constraints: keyboard and enclosure temperatures, motherboard bow, positioning after drop and vibration, and serviceability all matter. Whether a pad belongs on a CPU or GPU core is a structural-design decision. Do not treat it as an automatic replacement for the grease or phase-change interface in the original design.

 

Concept illustration of thermal interfaces on a storage device

 

Figure 5. Concept illustration of thermal interfaces on a storage device. The material form shows installation locations only; it does not identify a specific AF grade or a measured installation.

SSD vs HDD: Similar Shelf, Different Rules

An SSD has no read/write head or magnetic platter. Its concerns include controller and NAND temperatures, board-level material compatibility, and cleanliness around connectors. AF800 and AF1000 can be candidates for controller hotspots, with AF500 serving lower-heat areas — all subject to device-temperature and mechanical-pressure validation.

A mechanical hard drive has a different internal structure and its own cleanliness rules. Using AF material on the external control board is not the same application as placing material inside the drive cavity. Each requires separate structural and material approval.

Mobile and Communications Devices

Routers, wireless access points, mobile terminals, and communication modules can evaluate AF pads between main processors, RF power amplifiers, power components, and metal heat spreaders. A non-silicone formulation reduces one potential contamination source near camera modules, precision connectors, or relays. AF500 covers general gap-filling evaluations; AF800 and AF1000 address higher-conduction locations, with RF and insulation compatibility checked alongside thermal performance.

Automotive Control and Navigation

In ECUs, in-vehicle navigation, and cockpit electronics, control chips, power devices, and memory commonly conduct heat into metal housings. AF500 is a candidate for general control boards, while AF800 and AF1000 can be compared at localized high-heat devices. Near vehicle cameras and other optical parts, the non-silicone formulation also helps control a specific contamination pathway.

All three current TDS documents list −40 to 125 °C. Engine-compartment projects still need the actual maximum interface temperature plus validation against oils, coolant, damp heat, vibration, and thermal cycling. A temperature range on a TDS is not an automotive qualification.

BMS and BDU in Battery Packs

Inside a battery pack, BMS circuits, BDU power distribution, and switching components have different heat paths and electrical environments. Materials near relays or contactors deserve particular attention because emissions can affect contact systems. The AF Series is a candidate for reducing silicone sources, but the contactor's sealed construction and approved-material list still need separate review.

 

Concept layout of thermal interfaces on the bottom of a BDU

 

Figure 6. Concept layout of thermal interfaces on the bottom of a BDU. Purple marks interface locations; it is not the actual AF product color.

 

Start with AF500 for general board-level BMS cooling, then test AF800 and AF1000 at localized hotspots in the BDU or control unit. Place materials only in heat-transfer and insulation areas approved by the design, keeping them away from contacts, moving mechanisms, and connection surfaces.

Large cell-to-liquid-cold-plate interfaces bring their own checklist: compression reaction, thickness tolerance, areal density, cost, and automated assembly. High conductivity alone cannot make that decision. Electrical insulation, fire barriers, and thermal-runaway protection each require their own functional design.

One more boundary: AF1000's UL94 V-0 listing applies only to the 1–2 mm thickness stated in its TDS. It cannot be extended to 0.5 mm, and it does not replace pack-level fire or thermal-runaway-propagation validation.

AF500 Aging Record: Useful Evidence, With a Date Stamp

Long-running equipment needs evidence of how a material changes under heat, not just how it behaves on day one. An existing Sheen non-silicone product presentation records an internal AF500 reliability test: a 3.5 mm specimen aged at 110 °C for 1,008 hours, with conductivity and hardness recorded at each interval.

 

AF500 High-Temperature Aging Test Curve

 

Figure 7. Historical high-temperature aging conductivity record for one AF500 specimen, including all seven observation points.

 

Time, h01683365046728401008
Thermal conductivity, W/(m·K)3.353.293.253.283.303.263.27
Hardness, Shore 00483955494147.542

Table 3. Historical AF500 specimen: 3.5 mm initial thickness, aged at 110 °C for 1,008 hours. These readings describe the historical specimen, not current TDS limits.

 

The specimen moved from 3.35 to 3.27 W/(m·K), a final-to-initial retention of about 97.6%. Every conductivity reading stayed within the report's ±15% acceptance band relative to the initial value, and every hardness reading stayed within 48 ± 10 Shore 00.

Useful? Yes. A lifetime guarantee? No. This is historical evidence for one AF500 specimen. It does not replace validation of current production batches, justify a multi-year life prediction, or establish aging behavior for AF800 and AF1000.

Connect the Lab Record to Your Real Duty Cycle

During sample validation, retain the initial thickness, compression conditions, and thermal-test conditions. Add thermal cycling, damp heat, assembly retention, and bleed testing as the equipment environment requires. Silicone-sensitive structures should also include optical-window condensation, volatile-species analysis, or relay-compatibility observation, so thermal and cleanliness performance are judged under the same application conditions.

The chart comes from a 2025 internal historical report. Its initial conductivity, hardness, and specimen thickness differ from the current TDS table. Keep those specimen contexts separate; the historical values are not substitutes for current product specifications.

 

Cleanliness Validation: Test the Assembly, Not Just the Pad

A cleanliness requirement becomes useful only when it becomes measurable. ‘No intentionally added silicone in the formulation,’ ‘specified siloxanes not detected,’ and ‘no deposit observed on the assembled optical window’ answer three different questions. A non-silicone base helps with one route, but non-silicone volatiles, bleed products, and neighboring auxiliary materials still deserve attention.

Turn Cleanliness into Comparable Tests

 

EvaluationConditions and Metrics to RecordQuestion It Answers
Specified siloxane analysisTarget species; sampling or extraction method; detection and quantification limits; resultAre the specified siloxanes detected under the agreed method?
Optical-window condensation and surface depositionMaterial and window temperatures; distance; time; transmittance or haze change; surface photosDoes deposition affect optical function in the real structure?
Bleed under heat and pressureTemperature; pressure; contacting substrate; time; migrated area or mass; measurement methodDo bleed products migrate into sensitive areas?
Functional compatibility after assemblyDevice temperature; optical metrics; connection or switching function; retest timingCan thermal and cleanliness performance meet project requirements together?

Table 4. Recommended validation items only. They do not indicate that AF500, AF800, and AF1000 have already completed these tests. Acceptance limits belong to the project, and ‘not detected’ for specified species does not mean zero total volatiles.

Use Controls and Include Every Auxiliary Material

For optical-window deposition, include a blank control with no candidate pad. Keep temperature, time, installation distance, and sample quantity consistent across candidates, and add the incumbent material as a comparator where useful. Record optical metrics and surface condition before exposure, then retest under the agreed conditions. A quick visual glance is not a cleanliness method.

Control additional adhesive, release-liner residue, sealants, and assembly cleaning as part of the same experiment. If the delivered part includes an adhesive layer, include that layer in the test article. Vacuum equipment may separately specify TML and CVCM; ASTM E595 is a vacuum-outgassing method, not a direct substitute for optical-window compatibility testing in an atmospheric-pressure instrument.

What the Current Evidence Does — and Does Not — Establish

The current TDS documents support grade-parameter comparisons. The historical AF500 report supports observations of high-temperature aging for one specimen. Specified siloxane content, optical-window deposition, low-pressure thermal resistance, and compression curves for current grades should be discussed when requesting samples and completed through project testing where needed.

 

A Sensible First Sample Matrix

Start with a comparable sample set that tests thermal performance and assembly together. Then move the shortlisted grades into cleanliness and reliability validation. You do not need to choose a single winner in the first email, and you certainly do not need to choose AF1000 just because it has the highest conductivity.

 

CandidateExample Sample Size and ThicknessPurpose of First Comparison
AF500, 55 Shore 00 option20 × 20 × 1.0 mmGeneral thermal requirement and contact behavior
AF800, 70 Shore 0020 × 20 × 1.0 mmOverall performance with higher conductivity
AF1000, 70 ± 8 Shore 0020 × 20 × 1.0 mmReal benefit of the higher conductivity grade
AF500, 70 Shore 00 optionAdd the same size if neededCompare hardness options within the same grade

Table 5. Suggested sample requests only — not confirmed stock or delivery commitments. Match actual dimensions, thickness, and tolerances to the project. Quantity, cost, lead time, and available reports should be confirmed with Sheen.

 

Talk to Sheen About Your Structure

Contact Sheen Materials for AF500, AF800, and AF1000 selection support and die-cut samples. A useful first message is simple: ‘This is a component-to-housing interface in precision equipment. We need to evaluate cooling, compression load, and optical cleanliness together.’ Add requests for same-thickness thermal resistance, compression curves, and available emissions reports, and the discussion starts on engineering ground rather than adjectives.

Sheen Thermal

Manufacturer of thermal interface materials and silicone foam for automotive electronics, energy storage, power electronics, communications and consumer electronics.

Certified

  • ISO 9001:2015
  • ISO 14001:2015
  • IATF 16949:2016

What we supply

  • Thermal conductivity Up to 130 W/m·K
  • Thickness 0.3–10.0 mm
  • Custom & samples Die-cut to drawing, 3–7 days
Request a Quote