SF1600-BN Boron Nitride Pads: Selecting by the Assembled Interface
Date:2026-11-27
Power devices hand their heat to a metal heatsink or cold plate, and that same interface often has to keep electricity where it belongs. When the gap is already fixed and clamping force cannot simply go up, a conductivity number is not enough to choose a pad. Backing adhesive, compressed thickness and the state of the two contact faces all move the final interface ΔT. We built the SF1600-BN series for exactly this situation — but we would rather you judge it by what your own assembly measures than by 16 W/(m·K) on a datasheet.

Why 16 W/(m·K) Is Not the Answer
SF1600-BN uses hexagonal boron nitride filler in a silicone base. The family carries a nominal 16 W/(m·K) conductivity, per-thickness resistance and AC breakdown figures, plus pressure, recovery, adhesive and aging test data. Its value is not that one headline number; it is that an electrically insulating interface can now be screened against your real structure, thickness by thickness.
Units used throughout: area-normalized thermal resistance in K·cm²/W, which includes the effect of the tested contact interfaces. Measured results, TDS limits and worked examples are labelled separately — please do not let them trade places.

Figure 1. SF1600-BN product appearance and interface mating.
Four situations bring engineers to us most often. Each one has a different first check:
| Your selection problem | What SF1600-BN may offer | What to verify first |
|---|---|---|
| Conduct heat and isolate electricity at once | Evaluate the 16 W/(m·K) nominal conductivity together with per-thickness insulation figures | Resistance at the real gap, and insulation margin |
| Thickness fixed, temperature rise still high | Use pressure and resistance data to see whether contact can still improve | Interface ΔT within the allowed load |
| Pre-positioning needed, but resistance climbs | Compare no adhesive, dot-matrix adhesive and full-surface adhesive | Positioning effect and the added resistance |
| Samples work, production spec is hard to fix | Write compressed thickness, assembly conditions and post-aging re-test into the confirmed spec | Batch consistency and acceptance method |
[sample request link] If your project sits in one of these rows, tell us where the pad goes, how large the gap is and which problem you most want solved, and we will send matching samples. The first round has one job: decide whether SF1600-BN deserves a deeper look under your assembly conditions.
Notice how all four rows end at the same place — a resistance measured on an assembled interface. So let us start with the budget that resistance has to fit.
The Budget Comes First: Thickness, Insulation and ΔT
When one interface has to conduct heat and isolate electricity, thickness has to satisfy tolerance coverage, insulation margin and the thermal budget at the same time. The thin grades give us a starting point: the 0.3 mm TDS lists AC breakdown ≥4 kV and resistance ≤0.30 K·cm²/W, and the series performance report measured 0.286 K·cm²/W on a sample of the same nominal thickness at 40 psi and 80 °C.
| Nominal thickness (mm) | Mean compressed thickness (mm) | Mean measured resistance (K·cm²/W) | AC breakdown, corresponding TDS |
|---|---|---|---|
| 0.3 | 0.264 | 0.286 | ≥4 kV |
| 1.0 | 0.950 | 0.695 | ≥10 kV |
| 1.5 | 1.308 | 0.974 | ≥12 kV |
Table 1. Resistance tested on 25.4 mm × 25.4 mm specimens, three pieces per thickness, at 40 psi (≈275.8 kPa) and 80 °C.
Now let us turn that into a budget you can actually use. Suppose 100 W passes uniformly through a 4 cm² interface and you can allow 10 K across the pad and its contact faces. In a one-dimensional uniform approximation the allowable area-normalized resistance is 10 × 4 ÷ 100 = 0.40 K·cm²/W. Under Table 1's test conditions, the 0.3 mm sample gives about 7.15 K and can enter validation; the 1.0 mm sample gives about 17.38 K and the 1.5 mm about 24.35 K, so those two need a fresh look at thickness, effective contact area, or the whole cooling structure. These are calculated comparisons of different grades under one assumption, not measured chassis temperature rises.

Figure 2. Sheen thermal test equipment and specimens before and after testing.
This is where SF1600-BN earns its place: thermal design and insulation design can be screened at the same thickness. If your current difficulty is a large ΔT across an insulating interface, start with a thin grade that meets both the gap and the electrical requirement, then compare it with your existing material under identical conditions. Three boundaries travel with that advice:
- If the real gap is 1.0 mm, you cannot switch to 0.3 mm just to lower resistance.
- Data taken at 40 psi cannot stand in for results at a lower pressure.
- Breakdown voltage is a material screening figure, not a long-term working voltage — final thickness and insulation margin have to be confirmed against assembly damage risk, creepage distance, clearance and your product requirements.
But look again at Table 1: every measured value there was taken at 40 psi. Pressure is not a footnote. It is our next variable.
When the Gap Is Fixed, What Is Left Is Contact
Once the gap is fixed and the structure cannot accept a visible thickness change, a rising interface ΔT has two possible sources: the material itself, or the state of the contact faces. A combined pressure-and-resistance test helps you tell them apart. Here is a set of supplementary observations we think belongs in sample validation.
Separating bulk from contact
| Pressure (kPa) | Compressed thickness (mm) | Measured total resistance | Est. bulk resistance | Est. sum of two contact resistances | Contact share |
|---|---|---|---|---|---|
| 48.8 | 0.695 | 1.4100 | 0.3400 | 1.0700 | 75.89% |
| 95.8 | 0.695 | 1.0100 | 0.3400 | 0.6700 | 66.34% |
| 193.3 | 0.693 | 0.6100 | 0.3400 | 0.2700 | 44.26% |
| 241.5 | 0.693 | 0.5773 | 0.3400 | 0.2373 | 41.11% |
Table 2. All resistance values in K·cm²/W. Pressure, thickness and total resistance are supplementary measured values; bulk resistance is held at an approximate 0.34 and the two contact resistances are then estimated as a sum.

Figure 3. Resistance decomposition and pressure response of the same supplementary data set.
- Compressed thickness moves from 0.695 to 0.693 mm — roughly 0.29% — while total resistance falls from 1.4100 to 0.5773 K·cm²/W, about 59.1%.
- Within this sample and pressure range, that supports improving contact as a route to lower total resistance.
- It does not mean the assembly load was small, and it does not speak for every SF1600-BN grade.
Where the 0.34 estimate comes from
If bulk effective conductivity and contact conditions can be treated as roughly constant, area-normalized total resistance can be written as Ra = 10t/k + Rc, with t in mm, k in W/(m·K), and Ra and the sum of the two contact resistances Rc both in K·cm²/W. Fitting across different compressed thicknesses gives a slope and an intercept separately.

Figure 4. SF1600 Series Boron Nitride Thermal Pads Fitting across different compressed thicknesses.
Back to the practical question. From 193.3 to 241.5 kPa, total resistance falls by only 0.0327 K·cm²/W. For an ideal uniform 100 W / 4 cm² interface, ΔT moves from about 15.25 to 14.43 K while clamping force rises from about 77.3 to 96.6 N — roughly 19.3 N more for about 0.82 K. We suggest finding the point where the improvement starts to flatten, inside the load your device and PCB can actually accept, and setting assembly pressure there. If your clamping force cannot go up, test SF1600 at that pressure directly instead of borrowing a result from a higher one.
Pressure is one way an assembled interface changes. Adhesive backing is another — and it is chosen for a completely different reason.
Adhesive: Positioning Has a Thermal Price
Thin-sheet installation, cover-plate assembly and vertical mounting all benefit from pre-positioning. But adhesive also changes the heat-transfer interface. For projects that need it, we ran no-adhesive, dot-matrix adhesive and full-surface adhesive samples at the same thickness, so you can weigh assembly convenience against thermal performance.
| 2.0 mm specimen | 10 psi | 20 psi | 30 psi | 40 psi | 50 psi |
|---|---|---|---|---|---|
| No adhesive | 1.440 | 1.328 | 1.242 | 1.205 | 1.293 |
| Dot-matrix adhesive | 1.535 | 1.387 | 1.296 | 1.249 | 1.363 |
| Full-surface adhesive | 1.832 | 1.776 | 1.686 | 1.598 | 1.579 |
Table 3. Measured resistance from the adhesive comparison report, K·cm²/W. Test date 22 October 2026; the report states ASTM D5470.

Figure 5. Pressure response of samples at the same thickness with different adhesive forms.
At 30 psi on 2.0 mm samples, dot-matrix adhesive reads 1.296 K·cm²/W against 1.686 for full-surface — about 23.1% lower. No adhesive reads 1.242, so the dot version adds roughly 4.3%. If your project genuinely needs pre-positioning, both adhesive forms deserve a place in the first round. In the same report, 1.5 mm samples at 30 psi read 1.074 and 1.136 K·cm²/W, a gap of about 5.5%. The improvement changes with thickness and pressure, so please do not carry 23.1% over as a universal gain.
Build the first sample set around your real gap:
- Fix one thickness from the actual assembly gap.
- Keep a no-adhesive sample as the baseline.
- Add whichever adhesive form your assembly needs, at that same thickness.
- Beyond resistance, check positioning retention, shift after cover assembly, adhesive-layer compatibility and the rework process.
One more caution from this data set: the 2.0 mm no-adhesive and dot-adhesive samples show resistance rising again between 40 and 50 psi, so the pressure window needs repeat verification. This comparison describes our own samples; it is not a verdict on other brands' materials. The final choice has to satisfy installation and keep resistance acceptable at the same time.
Adhesive and pressure are assembly-day decisions. The next question is what happens to that same pad after months of load and heat.
Will It Still Hold After Assembly and Heat?
A gap-filling pad also has to keep assembly load under control. The SF1600-BN TDS lists Shore C hardness 50–70, and the compression curve for a 2.0 mm sample shows instantaneous assembly stress climbing with the compression target — from 18.60 psi at 10% deformation to 153.66 psi at 50%. 'Compressible' never means 'ignore the force on the device'.

Figure 6. Mean instantaneous compression stress of a 2.0 mm specimen. Specimens 25 mm × 25 mm, descent speed 0.5 mm/min, three tests per point.
In the same report, a 0.3 mm sample compressed 50%, held 30 minutes and left to recover 10 minutes after unloading returned an average recovery of 92%. That supports assemblies needing shape recovery, but your validation should watch compressed thickness, contact recovery and resistance together, and confirm the grade against its own recovery figure.
Then there is the long view. These are the questions we hear most, the evidence we already have, and what your project still has to confirm:
| Your long-term question | Existing test evidence | What your project should confirm |
|---|---|---|
| How does thermal performance change after high temperature? | 1.5 mm, 125 °C × 1000 h: resistance increased 14.2% | Build drift margin into the initial thermal budget and re-test under real conditions |
| Any exudation under compression and heat? | 1.0 mm oil exudation detail mean 1.28%; 2.0 mm batch D25 exudation rate mean ≈1.96%. Both at 50% compression, 125 °C × 1 week | Different specimens and internal methods were used separately; run compatibility checks at contamination-sensitive locations |
| How much mass does the material lose at high temperature? | 2.0 mm, 125 °C × 24 h: mean weight loss 0.27% | Evaluate weight loss separately from oil exudation and condensables |
Table 4. Reliability test specimens and conditions. The 1.0 mm exudation mean comes from the performance report detail table; the 2.0 mm exudation mean is calculated from two results in a separate exudation-rate report.
These figures let you define mechanical load and post-aging pass criteria at the sample stage, instead of measuring only the initial temperature rise and reworking later. SF1600-BN is silicone-based, so applications next to optical end faces, precision contacts or coated surfaces should treat migration, cleanliness and surface compatibility as separate validation items.
At this point every constraint is on the table — gap, insulation, pressure, adhesive, load and aging. We can finally shorten the candidate list.
Turning the Constraints Into a Shortlist
Fix the gap and the electrical isolation requirement first, then screen resistance and adhesive options. That order saves you from ordering too many grades and repeating tests. The SF1600-BN family has eight per-thickness TDS documents you can use to build a first-round list.
| Model | Nominal thickness (mm) | TDS resistance limit (K·cm²/W) | Test pressure | AC breakdown | Recovery |
|---|---|---|---|---|---|
| SF1600-BN-02 | 0.2 | ≤0.25 | 40 psi | ≥2 kV | ≥90% |
| SF1600-BN-03 | 0.3 | ≤0.30 | 40 psi | ≥4 kV | ≥90% |
| SF1600-BN-05 | 0.5 | ≤0.50 | 40 psi | ≥5 kV | ≥80% |
| SF1600-BN-07 | 0.7 | ≤0.70 | 40 psi | ≥6 kV | ≥70% |
| SF1600-BN-10 | 1.0 | ≤0.80 | 40 psi | ≥10 kV | ≥70% |
| SF1600-BN-15 | 1.5 | ≤1.10 | 40 psi | ≥12 kV | ≥60% |
| SF1600-BN-20 | 2.0 | ≤1.40 | 40 psi | ≥12 kV | ≥60% |
| SF1600-BN-30 | 3.0 | ≤1.70 | 30 psi | ≥12 kV | ≥60% |
Table 5. Compiled from the per-model TDS documents. The 3.0 mm resistance was tested at 30 psi; all other listed models at 40 psi.
A few material parameters belong in the same conversation: density 1.6 ± 0.2 g/cm³, relative permittivity ≤4.2 at 1 MHz, service temperature −40 to 150 °C, and V-0 flammability. Volume resistivity is ≥10¹³ Ω·cm for the listed grades at 0.3 mm and above, and ≥10¹² Ω·cm for 0.2 mm. High-frequency, long-term high-voltage or contamination-sensitive applications need their own confirmation at the relevant frequency, insulation system and environment.
Three kinds of projects are worth contacting us early:
- Power device to metal cold plate or heatsink, where electrical isolation is required and the thermal budget is tight — evaluate the matching thin grade first, and record device case temperature, cold-plate temperature, compressed thickness and insulation state together.
- Cover plate or chassis assembly that needs pre-positioning but cannot afford a large adhesive penalty — compare dot-matrix and full-surface adhesive at the same thickness, and decide by real-assembly shift and temperature rise together.
- Interfaces with controlled assembly height and adjustable clamping — use the pressure and resistance data to find a working window. For fragile devices or low-load structures, confirm the allowed total clamping force before testing at a given face pressure.
A shortlist is still paper. Whether it earns a place in your design is decided by one round of like-for-like comparison.
Make the First Round of Samples Answer One Question
Tell us where the pad goes, the assembly gap and the problem you most want to improve; then add allowed load and electrical requirements, and we can settle the candidate thickness and sample combination with you. Your current material tested under the same conditions is the most direct benchmark for replacement value.
| First-round focus | Suggested comparison method | The conclusion you need |
|---|---|---|
| Does the insulating interface ΔT improve? | At the same real gap, contact area, face pressure, temperature and surface state, compare your existing material with SF1600-BN | Whether the interface ΔT meets budget and insulation plus coverage pass |
| Is there still room to optimise pressure? | Choose pressure points only inside the device's allowed range; record total clamping force and compressed thickness | Whether more load buys enough thermal benefit |
| Is changing the adhesive worth it? | Compare the adhesive forms your project needs at the same thickness and pressure | Whether resistance, positioning retention and assembly process can all be satisfied |
| Will the performance survive service conditions? | After aging or cycling as your project requires, re-test resistance, insulation and appearance | Whether drift stays inside your acceptance range |
Table 6. First-round sample comparison suggestions. When comparing thickness, record both the nominal gap and the actual compressed thickness; final acceptance thresholds are set by the specific product design.
What we have shown here are SF1600-BN specifications, test cases and selection calculations. You choose the direction of validation; your own interface data decides whether to adopt it.
Once samples pass, write the validated conditions into the purchasing spec:
- Confirmed model, thickness and tolerance, die-cut dimensions and adhesive form.
- Inspection pressure and temperature, resistance requirement and batch traceability.
- Then confirm sheet size, MOQ, quotation, and sample and production lead times with us.
Purchasing then receives a supply condition that has already been validated, which cuts the interpretation gap between engineering and supply.
Data source:
- [1] Sheen SF1600-BN-02 / 03 / 05 / 07 / 10 / 15 / 20 / 30 TDS — eight per-thickness TDS documents, page 1 of each.
- [2] Sheen, SF1600-BN Series Performance Test Report, proposed date 4 August 2025.
- [3] Sheen, SF1600-BN-A1 Dot-Matrix Adhesive vs Full-Surface Adhesive Comparison Test Report, test date 22 October 2026.
- [4] Sheen, SF1600-BN Oil Exudation Rate Test Report, 26 October 2026, 2.0 mm, batch D25.
- [5] Supplementary thickness–resistance fit chart, ~0.7 mm specimen pressure / thickness / resistance table, contact resistance vs pressure chart and notes.
- [6] ASTM International, ASTM D5470-17(2024) public description 5.1–5.4.1, https://store.astm.org/d5470-17r24.html, accessed 27 November 2026.
[Contact us] for SF1600-BN boron nitride thermal pad samples together with the corresponding TDS, pressure–resistance data and adhesive comparison material, and let the first round of testing decide whether it improves your insulating thermal interface.
We started by saying 16 W/(m·K) is not the answer. It is the starting point. What decides your design is the ΔT you measure at your own gap, pressure, insulation margin and assembled state — and whether that number is still there after adhesive, load and heat have had their say.
Sheen Thermal
Dongguan Sheen Electronic Technology Co., Ltd · Founded in 2008
Manufacturer of thermal interface materials and silicone foam for automotive electronics, energy storage, power electronics, communications and consumer electronics.
Certified
- ISO 9001:2015
- ISO 14001:2015
- IATF 16949:2016
What we supply
- Thermal conductivity Up to 130 W/m·K
- Thickness 0.3–10.0 mm
- Custom & samples Die-cut to drawing, 3–7 days